MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Abatron AboCast 8103-16 One Part Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: One component system. Less viscous than 8103-11. Information provided by Abatron, Inc.

Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 360 min. at 100°C (212°C). Peak exotherm 130°C (265°F). At 100°C (212°F), gels in 3-4 hrs, total cure in 4-6 hrs. At 110-120°C (230-250°F) gels to 0.5-1 hr and total cure in 1-2 hrs.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 1500
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 87
Tensile Strength, Ultimate 47.78 MPa
Elongation at Break 14.4 %
Flexural Yield Strength 73.02 MPa
Flexural Modulus 2.12 GPa
Compressive Yield Strength 68.95 MPa
Compressive Modulus 2.21 GPa
Izod Impact, Notched 0.368 J/cm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 7.52e+14 ohm-cm
Surface Resistance 4.71e+14 ohm
Dielectric Constant 3.13
@Frequency 1e+6 Hz
 3.4
@Frequency 1000 Hz
 3.46
@Frequency 60 Hz
Dissipation Factor 0.0044
@Frequency 60 Hz
 0.012
@Frequency 1000 Hz
 0.024
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 62.0 °CDeflection temperature; load unknown.
 
Processing PropertiesOriginal ValueComments
Pot Life 360 min
@Temperature 360 °C
500 g
 
Descriptive Properties
Exotherm130°CPeak

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plenco 2308 Phenolic, Granular, Injection Molded
Overview of materials for Acrylic, Extruded
Bakelite® UP 3720 Unsaturated Polyester Resin, UL Listed, Low Shrinkage, High Arc Resistance
Bakelite® PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof

PABEN1 / 22014

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.