Petrothene LB500302 is a polyethylene resin that exhibits excellent environmental stress crack resistance and is selected by customers for use in heavy duty bottles, such as those containing detergent and chemicals. Availability: North America Application: Bottles For Consumer Goods; Bottles for Industrial Use Market: Rigid Packaging Processing Method: Extrusion Blow Molding Attribute: Good ESCR (Environmental Stress Cracking Resistance) Information provided by LyondellBasell. |