MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep. The resin shows outstanding bubble stability.

Main Applications: Greenflex FC 45 is recommended for the production of very wide agricultural films.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.935 g/ccISO 1183
Vinyl Acetate Content 14 %Internal Method
Thickness 50.0 - 200 micronsRecommended
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ISO 868/A
Hardness, Shore D 40ISO 868/A
Film Tensile Strength at Yield, MD 5.00 MPaISO 527-3
Film Tensile Strength at Yield, TD 4.00 MPaISO 527-3
Film Elongation at Break, MD 490 %ISO 527-3
Film Elongation at Break, TD 650 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50ISO 8295
Elmendorf Tear Strength, MD 2.4456 g/micronISO 6383-2
Elmendorf Tear Strength, TD 4.076 g/micronISO 6383-2
Dart Drop Test >= 700 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 30.0 MPaISO 527-3
Film Tensile Strength at Break, TD 30.0 MPaISO 527-3
1% Secant Modulus, MD 65.0 MPaISO 527-3
1% Secant Modulus, TD 70.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 93.0 °CInternal Method
Vicat Softening Point 73.0 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -80.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %ISO 14782
Gloss 80 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Versalis Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
BASF Ultraform® N2200 G43 POM
Versalis Clearflex® FG B0 Very Low Density Polyethylene
Versalis Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding

PENG133 / 124527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.