MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Corr-Paint™ CP4000-S2-HT High Temperature Silicone-Glass-Ceramic Protective Coating
Categories: Ceramic; Glass; Glass Ceramic; Polymer; Thermoset; Silicone

Material Notes: Single part, low viscosity, room temperature curing, flame resistant, dielectric, silicone-glass-ceramic sealer offering continuous temperature resistance to 1500°F (816°C) and intermittent resistance to 1800°F (982°C).

Vendors: Aremco offers a broad range of coatings formulated using an advanced solvent-based silicone resin combined with inorganic fillers and pigments. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/cc
Solids Content 70 %Volume
 73 %Weight
Volatiles 18.3 %
Viscosity 150 - 500 cP
Thickness 25.4 micronsDry Film Thickness
 115 micronsWet Film Thickness
Storage Temperature 40.0 - 90.0 °F
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1400 °CContinuous
 1800 °FIntermittent
Flash Point 113 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 90.0 °FApplication Temperature
Dry Time >= 1.00 hourCuring, Min Air Set
 1.00 - 2.00 hourTouch
 2.00 - 4.00 hourHandling
 1.00 - 24.0 hourRecoat
Cure Time 24.0 - 48.0 hour
@Temperature 22.8 °C
or 450°F / 1 hr
Shelf Life 3.00 Month
 
Descriptive Properties
ColorBlack
Theoretical Dry Film Coverage, ft2/gal1122
ThinnerT-Butyl Acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ZPAREM963 / 316323

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.