Typical applications: - V-belts
- Shoes
- Printing rolls
Advantages: - Better tensile properties than NBR
- Higher continuous service temperature
- Good chemical resistance
- Improved tear and abrasion properties than NBR
Disadvantages: - Not suitable for brake fluids, ketones, strong acids or phosphate esters
- Poor resistance to ozone and weathering
- Higher compression set
Information provided by CLWYD COMPOUNDERS LTD. |