FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, and high puncture resistance and are readily heat sealable. Addition of slip and antiblock agents should be considered for most applications. Information provided by Dow |