MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 30%Glass Fiber Filled

Material Notes: Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the material, while maintaining most of its other basic characteristics. The combination of structural properties and cost effectiveness make this resin an attractive alternative to metals in many engineering applications.

Features: Acid Resistant; Flame Retardant; Good Adhesion; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Rigidity; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight

Uses: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Applications; Metal Replacement; Microwave Cookware; Plumbing Parts; Valves/Valve Parts

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccASTM D792
Filler Content 30 %Glass Fiber
Water Absorption 0.40 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 343 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 130 MPaASTM D638
Elongation at Break 1.9 %ASTM D638
Tensile Modulus 8620 MPaASTM D638
Flexural Strength 179 MPaASTM D790
Flexural Modulus 8620 MPaASTM D790
Izod Impact, Notched 75.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 4.11
@Frequency 60 Hz
ASTM D150
 4.13
@Frequency 1000 Hz
ASTM D150
 4.17
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.0018
@Frequency 1000 Hz
ASTM D150
 0.0019
@Frequency 60 Hz
ASTM D150
 0.0094
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
Deflection Temperature at 1.8 MPa (264 psi) 216 °CUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.787 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 343 - 399 °C
Mold Temperature 149 - 163 °C
Drying Temperature 149 - 177 °C
@Time 9000 - 14400 sec
 
Compliance PropertiesOriginal ValueComments
NSF YesNSF 61
 
Descriptive Properties
Agency RatingsNSF 61
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorColors Available; Opaque
FormPellets
Injection RateFast
Processing TechniqueInjection Molding
RoHS ComplianceRoHS Compliant
Screw Compression Ratio2.0:1.0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Akro-Plastic Akrotek® PEEK CF 40 black (5099) PEEK, Conditioned, 30% Carbon Filled

PSOL8Y7393 / 177124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.