MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Syncon® Premium EP Gear Oil, ISO Grade 320, AGMA Grade 6 EP
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Phillips 66® Syncon Premium EP Gear Oil is a premium quality, synthetic, extreme-pressure gear lubricant specifically recommended for lubricating the heavily loaded gears and rolling-element bearings in motorized wheel gearboxes found on mining haul trucks. It also is recommended for lubrication of enclosed industrial gear drives operating at extreme temperatures. Syncon Premium EP Gear Oil is formulated with synthetic polyalphaolefin (PAO) base oils, a non-chlorinated extreme-pressure additive and select inhibitors. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It has high load-carrying capacity to protect against scuffing and wear, protects against rust and corrosion, and is resistant to excessive foaming that can interfere with proper lubrication. Syncon Premium EP Gear Oil meets the performance requirements of General Electric Transportation Systems Specification D50E27. It is approved for use in GE AC and DC electric motorized wheel gearboxes found on Komatsu, Terex, Euclid and Hitachi mining haul trucks.

Applications:

  • GE motorized wheels found on mining haul trucks
  • Enclosed industrial gear drives operating at very high or very low temperatures, or operating continuously at higher than normal operating temperatures (1)
  • Heavily loaded plain and rolling-element bearings operating at extreme Temperatures
  • Applications where the equipment manufacturer recommends a synthetic extreme-pressure gear oil Syncon Premium EP Gear Oil meets the requirements of the following industry and OEM specifications:
    • ANSI/AGMA Standard 9005-E02, Anti-Scuff/Anti-Wear (EP) Oils
    • DIN 51517 Part 3, Lubricating Oils, Type CLP HC
    • GE Specification D50E27 (approved)
    • German Steel Industry SEB 181226, Type CLP HC
    • ISO 12925-1:1996, Type L-CKC
    • Joy Machinery Specification TO-SHEP (ISO VG 320)
    • U.S. Steel 224
    Features/Benefits:
    • Outstanding oxidation resistance and thermal stability at high temperatures
    • Outstanding low-temperature properties
    • High load-carrying capacity
    • Protects against scuffing and wear
    • Protects against rust and corrosion
    • Non-chlorinated additive system
    • Suitable for year-round use
    • Extended service intervals compared to conventional mineral oil-based gear oils

    Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.877 g/cc0.877 g/cc
Density 0.875 g/cc0.0316 lb/in³
Viscosity Measurement 123123Index
Saybolt Viscosity at 100°F 1682 SUS1682 SUS
Saybolt Viscosity at 210°F 142 SUS142 SUS
Kinematic Viscosity at 40°C (104°F) 320 cSt320 cSt
Kinematic Viscosity at 100°C (212°F) 29 cSt29 cSt
ASTM Color 1.01.0ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.400.40[mg KOH/g]; ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2596
Four Ball Wear 0.360 mm0.0142 inScar Diameter; ASTM D4172
Timken Test >= 27200 g>= 60.0 lbOK Load; ASTM D2782
 
Thermal PropertiesMetricEnglishComments
Pour Point -34.0 °C-29.2 °F
Flash Point 238 °C460 °FCOC
 
Descriptive Properties
Copper Corrosion1bASTM D130
FZG Scuffing Test>12 Failure Load StageASTM D5182
Oxidation Stability<4%Viscosity Increase @ 121°C, ASTM D2893

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5103 / 198356

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.