MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reade Advanced Materials Indium-Tin Oxide (ITO) Powder (In2O3:SnO2)
Categories: Ceramic; Oxide

Material Notes: 99.99% (metals basis). Indium oxide doped with tin oxide, ITO, is used to make transparent conductive coatings. Thin film layers can be deposited by electron-beam evaporation or sputtering. Roll or web coating on polymer substrates is done by magnetron or other techniques of sputtering. End uses of ITO are: Flat panel displays; ITO glass manufacturing techniques; electroluminescent displays; plasma display panels; electrochromic displays; field emission displays; and heat reflecting mirrors. Vacuum Deposition Grade is 99.999% purity metals basis.

Information provided by Reade Advanced Materials.

Key Words: In2O3:SnO2, Indium tin oxide
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.20 g/cc
Bulk Density 0.800 g/ccTap Denisty - Fine Grade
 0.500 - 1.20 g/ccApparent
 1.60 g/ccTap Denisty - Standard Grade
Particle Size 1 - 3 µmd50, Fine Grade
 12 - 18 µmd50, Standard Grade
Specific Surface Area 2.0 - 3.0 m²/gStandard Grade
 19.2 m²/gFine Grade
Molecular Weight 264.94 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 1900 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
CAS Number50926-11-9
Colorgreenish yellow
In2O390 wt%
SnO10 wt%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott Transparent ITO Conducting Oxide Coating
Indium Corp. Fine ITO Indium Tin Oxide
Indium Corp. Standard ITO Indium Tin Oxide
Tin, Sn
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window

CREADE014 / 1948

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.