MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrene-Butadiene Copolymer

Customer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent clarity, good toughness, excellent stiffness, high surface gloss, and can be blended with Polystyrene.

Applications: Garment Hangers

Processing Recommendations:
Melt Temperature: 232°C, maximum. Screw: plasticizing type injection molder more desirable than plunger type molder. Generally no need to dry resin.

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccASTM D792
Water Absorption 0.090 %ASTM D570
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 26.0 MPa2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 160 %2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 34.0 MPaTest specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 1.413 GPaTest specimens were injection molded by ASTM D1897; ASTM D790
Izod Impact, Notched 0.410 J/cm
@Thickness 3.17 mm
ASTM D256
Impact Test 29.7 J
@Thickness 3.17 mm
Instrumented Total Energy; @ 150 in/sec impact rate; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °CASTM D648
Vicat Softening Point 87.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 232 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade
Chevron Phillips K-Resin® CK02 Styrene-Butadiene Copolymer, Blow Molding Grade
Chevron Phillips K-Resin® BK18 Styrene-Butadiene Copolymer
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade

PCHEVK75 / 20288

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.