MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Ryton® XK3340 PPS Alloy
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Ryton® XK3340 is a 40% glass fiber reinforced polyphenylene sulfide alloy compound that provides good mechanical strength and stiffness along with low molding flash and excellent resistance to engine coolants (glycol/water) at elevated temperatures.

Applications: Automotive Applications

Features: Good Flow; Good Strength; Good Thermal Stability; Good Toughness; High Rigidity; Hydrolytically Stable; Low to No Water Absorption; Minimal Flash; Ultra High Glycol Resistance

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage, Flow 0.0089 cm/cm0.0089 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 175 MPa25400 psiISO 527-2
Elongation at Break 1.3 %1.3 %ISO 527-2
Tensile Modulus 16.0 GPa2320 ksiISO 527-2
Flexural Strength 223 MPa32300 psiISO 178
Flexural Modulus 15.7 GPa2280 ksiISO 178
Charpy Impact Unnotched 2.90 J/cm²13.8 ft-lb/in²ISO 179
Charpy Impact, Notched 0.880 J/cm²4.19 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.50e+16 ohm-cm4.50e+16 ohm-cmASTM D257
Comparative Tracking Index 262 V262 VUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 286 °C547 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 340 °C590 - 644 °FInjection
Mold Temperature 135 - 150 °C275 - 302 °F
Drying Temperature 120 - 135 °C
@Time 14400 sec
248 - 275 °F
@Time 4.00 hour
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4464 / 280264

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.