MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Chockfast® SUPER ALLOY Titanium Repair Compound Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: SUPER ALLOY Titanium Repair Compound is the latest in high technology, high bond strength repair systems. The SUPER ALLOY system was conceived through a program utilizing "state-of-the-art" computer science and systematic evaluations. Long, intensive studies resulted in SUPER ALLOY'S specific formulation providing industry with a fast, permanent repair to equipment that might otherwise require costly "downtime." The SUPER ALLOY system is the ideal solution to joining such dissimilar metals as iron, steel, aluminum, tungsten carbide, brass, zinc, and zinc alloys without the problems of galvanic corrosion.

USE & BENEFITS: • SUPER ALLOY adheres tenaciously to properly prepared surfaces. • SUPER ALLOY's advanced capabilities allow expedient repairs of castings, blocks, foundations, shafts and other equipment without the use of heat, pressure or special tools. The material hardens to a rigid metallic mass which permits drilling, tapping, or machining with ordinary metalworking tools. • Super ALLOY creates an integral bond, maintaining a high level of resistance to impact, abrasion, chemicals and high temperature.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787ASTM D1076
Flexural Strength 53.1 MPa7700 psiASTM C790
Compressive Strength 105 MPa15200 psiASTM C695
Adhesive Bond Strength 13.8 MPa2000 psiAdhesive Tensile Shear; ASTM D1002
Taber Abrasion, mg/1000 Cycles 2020Federal Test Standard 406
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.2 µm/m-°C40.1 µin/in-°FASTM D698
Maximum Service Temperature, Air 121 °C250 °F
Shrinkage 0.10 %0.10 %Linear; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time 1080 min
@Temperature 22.0 °C
18.0 hour
@Temperature 71.6 °F
approximate
Pot Life 25.0 min
@Temperature 22.2 °C
25.0 min
@Temperature 72.0 °F
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Colorgrayhardener
 graymixed
 silverresin
Mix Ratio by volume3 to 1Resin to hardener
Mix Ratio by weight4.3 to 1Resin to hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWC9034 / 239544

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.