MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTAMELT® 970 Copolyamide hotmelt adhesive  (discontinued **)
Categories: Polymer; Adhesive

Material Notes: VESTAMELT 970 is a copolyamide hot melt adhesive with good washing resistance. VESTAMELT 970 can be added to low viscous grades and the powder improves the resistance to strike back in pastes. VESTAMELT 970 is suitable for the manufacturing of films. Fields of application:
  • paste dot (base)
  • powder dot

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1.7 cPR307
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 160 °C
ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 116 °CISO 11357
 119 °CISO 3146

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6
Overview of materials for Thermoset Polyurethane, Adhesive
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
BASF Capron® 8200 NL Nylon 6 (DAM)
Aptek 3101 B/C/B Thermally conductive urethane film adhesive

PEVONIL300 / 196504

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.