MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Taiwan PU MPU60 Millable Polyurethane Rubber
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Key features:
  • Hardness: 50-90A
  • Appearance: White to cream color solid
  • Can be processed by conventional rubber manufacturing equipment
  • Harmless to human beings
Application: Seal, seal material. mechanical shock buffer material and parts of electronics industries and so on.

Introduction: UR SERIES is Polyester urethane rubber, which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of conventional rubber manufacturing equipment and techniques to yield finished urethane parts.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/cc
Mooney Viscosity 35 - 65
@Temperature 100 °C
35 - 65
@Temperature 212 °F
ML 1-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060
Tensile Strength 23.2 MPa3360 psi
Elongation at Break 640 %640 %
300% Modulus 4.00 MPa580 psi
Tear Strength 38.6 kN/m220 pliDie C
Compression Set 62 %
@Temperature 70.0 °C,
Time 79200 sec
62 %
@Temperature 158 °F,
Time 22.0 hour
 
Descriptive Properties
AppearanceSolid
ColorWhite to cream

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU059 / 305789

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.