MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
OCSiAl TUBALL™ MATRIX 601 Graphene Nanotube Concentrate
Categories: Carbon; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TUBALL™ MATRIX is a line of concentrates based on TUBALL™ graphene nanotubes (GNT) produced by OCSiAl. TUBALL™ MATRIX concentrates are available in several matrixes, are easy to handle, and can be processed using standard equipment. Depending on the TUBALL™ MATRIX percentage in the final compound and the processing conditions and other system components, the volume resistivity can be adjusted within the range from 10 to 108 Ohm·cm. TUBALL™ is a unique GNT additive that provides electrical conductivity at low dosages not achievable with any standard conductive additive. These low dosages enable the electrical resistivity of the material to be reduced with minimal impact on the host matrix, including retaining and even improving mechanical properties, minimally increasing the density, and limiting any influence on the rheological properties and color.

Benefits: TUBALL™ GNT, carried by TUBALL™ MATRIX, enable ultra-low dosage of conductive filler starting from just 0.03 wt.% for anti-static, static dissipative and conductive applications, Allow production of conductive parts that retain bright colors, Ensure permanent and uniform electrical conductivity without “hot spots”, Maintain rheology of the uncured compound, Standard processing and mixing equipment, Minimal influence on mechanical properties including softness.

Information provided by OCSiAl

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccDN 51757
 
Descriptive Properties
AppearanceBlack paste
CarrierPolydimethylsiloxane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EOCSIAL917 / 305656

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.