MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Total 3829 Polypropylene, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Easy flow LTHA injection molding homopolymer

Easy Flow - FINA 3829 exhibits exceptionally easy flow combined with physical properties similar to 4.0 melt polypropylene homopolymer.

UL Rating - FINA 3829 has a UL rating at 120oC (248o F)

FDA - FINA 3829 complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 3829 is recommended for appliance parts and is particularly suited for parts that are exposed to a hot/wet environment.

Processing - FINA 3829 resin processes on conventional injection molding equipment with typical melt temperatures of 350-450°F (177-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 30 g/10 min30 g/10 minASTM D1238L
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ASTM D288A
Tensile Strength, Ultimate 32.4 MPa4700 psiASTM D638
Elongation at Break 7.0 %7.0 %ASTM D638
Modulus of Elasticity 1.38 GPa200 ksiASTM D638
Flexural Modulus 1.17 GPa170 ksiASTM D790
Izod Impact, Notched 0.214 J/cm0.401 ft-lb/inASTM D256A
Izod Impact, Unnotched 8.55 J/cm16.0 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FDSC
Maximum Service Temperature, Air 120 °C248 °FUL Rating
Deflection Temperature at 0.46 MPa (66 psi) 121 °C250 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 - 232 °C351 - 450 °FInjection

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HL504FB Polypropylene Homopolymer
A. Schulman PP 829-01 Polypropylene Homopolymer Polypropylene
A. Schulman PP 3476 Polypropylene Homopolymer, Fiber Grade
Total 7823MZ Polypropylene, Injection Molding Grade
Total 7235 Polypropylene, Blow Molding Grade

PFIN32 / 38362

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.