MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM Cat Blue Condensation Cure Moldmaking Catalyst
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM Cat Blue is one of the catalysts for the QM 100 series of products. This is a two-component, room temperature, condensation cure system. The cured rubber has excellent mechanical properties and good shelf-life stability. QM Cat Blue catalyst is recommended for applications where long work life is essential. QM Cat Purple catalyst is available for applications requiring standard curing times. QM Cat Red 3 catalyst is available for applications that require very quick curing times. Thixotropic and styrene resistant catalysts are also available.

Key Features:

  • Long work life
  • 24 hour demold time
  • Excellent physical properties
Main Applications:
  • Molds for polyester and polyurethane resin castings
  • Molds where hand mixing is required
  • Glove molding applications

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccUncatalyzed
Viscosity 100 cPUncatalyzed
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 - 24.0 hourDemold time, Catalyzed
Tack-Free Time 6.00 - 8.00 hourCatalyzed
Pot Life 50.0 minCatalyzed
 
Descriptive Properties
ColorBlueUncatalyzed
 Light BlueCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PACC2062 / 199450

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.