MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccResin Density
 2.25 g/ccFiber Density
Filler Content 53.0 %Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 377 MPa90º, RT, Dry; EN2561
Tensile Modulus 28.0 GPa90º, RT, Dry; EN2561
Compressive Yield Strength 370 MPa
@Temperature 150 °C
90º, Wet; EN2850 Type B
Shear Modulus 3.00 GPaIn-Plane, RT, Dry; EN6031
 2.00 GPa
@Temperature 130 °C
In-Plane, Wet; EN6031
Shear Strength 48.0 MPa0º, ILSS Short Beam, RT, Dry; EN2563
 108 MPaIn-Plane, RT, Dry; EN6031
 27.0 MPa
@Temperature 150 °C
0º, ILSS Short Beam, Wet; EN2563
 32.0 MPa
@Temperature 135 °C
0º, ILSS Short Beam, Wet; EN2563
 58.0 MPa
@Temperature 150 °C
In-Plane, Wet; EN6031
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 - 130 °CEpoxy Matrix Limit
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
Cured Thickness per Ply (cm)0.011

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber
Solvay Thornel® P-120 Carbon Fiber/Epoxy Advanced Composite System
Hexcel® Fibrelam® 2000 Grade 5 Panels for Aircraft Flooring
Hexcel® Fibrelam® 2000 Grade 1 Panels for Aircraft Flooring

PHEXC184 / 98655

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.