MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chemours Krytox® XHT-ACX PFPE Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE); PTFE Gellant

Material Notes: The Krytox® XHT-AC series greases are an extension of the Krytox® 240 series and Krytox® GPL 22X series but are designed to give higher performance in the 204–302 °C (400–575 °F) ranges. Krytox® XHT-AC series greases contain sodium nitrite to offer anti-corrosion performance. These greases should be used below 320 °C (608 °F), where the PTFE thickener could begin to melt. The base oil is an extremely viscous oil that provides good viscosity and lower evaporation at high temperatures.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.99 g/cc
@Temperature 0.000 °C
Volatiles <= 0.75 %
@Temperature 204 °C,
Time 79200 sec
Viscosity Measurement 158Base Oil Viscosity Index
Kinematic Viscosity 2610 cSt
@Temperature 20.0 °C
Base Oil
Kinematic Viscosity at 40°C (104°F) 738 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 65 cStBase Oil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °C
Minimum Service Temperature, Air <= -10.0 °C
Pour Point <= -15.0 °CBase Oil
 
Descriptive Properties
Antirust Rating, ASTM D-1743Passes
AppearanceWhite, creamy consistency
Food Contact ApprovalNSF H-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Krytox® XHT-AC PFPE Grease
Chemours Krytox® NRT 8904 PFPE Lubricant
Chemours Krytox® XHT-BD Performance PFPE Lubricant
Chemours Krytox® CORR 226 FG PFPE Corrugator Grease
Chemours Krytox® XP 2A0 PFPE Grease

WDUPJ918 / 162452

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.