MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems Accura® CeraMAX™ Plastic for SLA® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Features:
  • Highest stiffness available
  • Heat and abrasion resistant
  • Excellent chemical resistance
  • Great for windtunnel models, jigs and fixtures

Information provided by 3D Systems

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccLiquid
 1.62 g/ccSolid
Viscosity 1500 - 2000 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89
Tensile Strength 78.0 - 87.0 MPaASTM D 638
Elongation at Break 1.0 - 1.5 %ASTM D 638
Tensile Modulus 9460 - 9680 MPaASTM D 638
Flexural Strength 137 - 145 MPaASTM D 790
Flexural Modulus 8270 - 8370 MPaASTM D 790
Izod Impact, Notched 14.5 - 17.9 J/mASTM D 256
Penetration 5.7[mils]
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.1 µm/m-°C
@Temperature 25.0 - 57.0 °C
ASTM E 831-93
 87.4 µm/m-°C
@Temperature 70.0 - 200 °C
ASTM E 831-93
Deflection Temperature at 0.46 MPa (66 psi) 148 °CUV Postcure Only; ASTM D 648
 220 °CUV + thermal postcure (2hr @ 120 °C); ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CUV Postcure Only; ASTM D 648
 97.0 °CUV + thermal postcure (2hr @ 120 °C); ASTM D 648
Glass Transition Temp, Tg 82.0 °CUV Postcure Only
 94.0 °C120 °C thermal postcure
 
Descriptive Properties
ColorWhite
Critical Exposure (Ec)7.2 mJ/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Mold Steel
Prodways PLASTCure ABS 3650 3D Printing Polymer
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
Clariant Natural Polycarbonate 3D Printer Filament
Aluminum 6061-T6; 6061-T651

PAPPR3104 / 239072

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.