MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
American Port Orford Cedar Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Sometimes known as Port Oxford Cedar. Softwood. Easy to work with hand tools. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Chamaecyparis lawsoniana; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.400 g/ccOven Dry Weight/Unseasoned Volume
 36.0 lb/ft³Unseasoned*
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 2100 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2500 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 240 psiPerpendicular to Grain*
Modulus of Rupture 0.0780 GPaIn Bending
 6.80 ksiStatic Bending*
Flexural Yield Strength 53.1 MPaBending stress at proportional limit
 3900 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 9.00 GPaIn Bending
 1500 ksiStatic Bending*
Compressive Strength 44.8 MPaParallel to Grain
 380 psiPerpendicular to Grain*
 2970 psiParallel to Grain*
 3280 psiMax Crushing Strength Parallel to Grain*
Shear Strength 880 psiParallel to Grain*
Impact 2.7in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 9300psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.590 in-lb/in³Static Bending*
Work to Maximum Load 7.80 in-lb/in³Static Bending*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.710 BTU-in/hr-ft²-°FOven Dry
 0.850 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.6 %Radial; Unseasoned to Oven Dry*
 6.9 %Tangential; Unseasoned to Oven Dry*
 10.6 %Volumetric; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Eastern Red Cedar Wood
American Alaska Cedar (Yellow Cedar) Wood
American Cedar Wood
American Pine Wood
American Red Spruce Wood

PTSAA / 71284

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.