MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem Wiraten 95 Polyethylene Wax
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Wiraten 95 is a low molecular weight polyethylene wax used as a process aid in a wide variety of polymer systems. Its outstanding compatibility and excellent flow and release characteristics make Wiraten 95 useful in almost every rubber compound. This product provides a lower softening point than standard PE wax.

Applications: Wiraten 95 finds use in rubber and plastic compounding, color concentrates, as an external vinyl lubricant and in hot melt adhesives. Wiraten 95 may be used to: improve flow for injection and transfer molding, provide release from hot metal surfaces (internal mixers, hot calendar rolls, extruder dies, and molds); improve filler dispersion when added early in mix; at higher loadings (>5phr), provide a glossier finish to cured parts. Wiraten 95 is typically used at the 2-6 phr level in virtually all elastomers (1 phr is the usual recommendation for fluoroelastomers). It provides release with minimal interference with adhesion properties. Note: for any PE wax to be effective it must be above melt point. Thus, PE waxes provide no release from mills but outstanding release from internal mixers and molds. Normally up to 5 phr may be added to a compound with little effect on vulcanized properties. High loadings (up to 20 phr) can be used in EPDMs to achieve high durometer non-black stocks that process well. Wiraten 95 should be melted when dispersed in a compound to prevent molding flaws (streaky blisters are evidence of lack of melt). Wiraten 95's lower softening point can provide release from equipment at lower processing temperatures. For example, the temperature at which a stock releases from a calendar or an internal mixer might be lowered 10°C (say from 120°C to 110°C), thus reducing stock heat history

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.925 g/cc0.925 g/cc
 
Mechanical PropertiesMetricEnglishComments
Penetration 12 - 1812 - 18[dmm]; ASTM D-1321
 
Thermal PropertiesMetricEnglishComments
Softening Point 85.0 - 95.0 °C185 - 203 °FASTM E28-97
Dropping Point 110 - 112 °C230 - 234 °FASTM D127
 
Descriptive Properties
Appearancewhite prill

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH645 / 315563

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.