MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Exact ™ 9182 Ethylene Alpha Olefin Copolymer
Categories: Polymer; Thermoplastic

Material Notes: Plastomers are ethylene alpha olefin copolymers that bridge the gap between elastomers and plastics. With rubber-like properties and the processability of plastic, they are used as polymer modifiers to provide unique properties in flexible packaging, molded and extruded products, and foamed compounds.  Benefits:  Flexible packaging – enhanced toughness, clarity and sealing performance, Molded and extruded products – improved impact strength and flexibility, Foamed compounds – added durability to lightweight shoe mid soles  With characteristics that improve strength and flexibility, Exact plastomer resins’ rubber-like properties support product durability and processability.  Exact 9182 is an ethylene butene copolymer produced using ExxonMobil's proprietary metallocene catalyst technology.  This resin is compatible with polyolefins like polypropylene, polyethylene, and ethylene-vinyl acetate copolymer resin. 

Availability:  Asia Pacific (* product may not be available in one or more countries in the identified availability regions.  Contact your sales rep for complete country availability.)

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.885 g/ccExxonMobil Method
Melt Flow 1.2 g/10 minExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 86ASTM D2240
Tensile Strength at Break >= 1400 psiASTM D412
Elongation at Break 440 %ASTM D412
100% Modulus 695 psi
@Strain 100 %
ASTM D412
Flexural Modulus, 1% Secant 5600 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 156 °FPeak; ExxonMobil Method
Crystallization Temperature 127 °FExxonMobil Method
Vicat Softening Point 160 °FExxonMobil Method
Glass Transition Temp, Tg -42.0 °FExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98952 / 238333

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.