MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Biphenyl Process Fluid
Categories: Fluid

Material Notes: Product Description: Applications for biphenyl process fluid include process media or solvents in many industries, including chemicals and petrochemicals.

Application/Uses:

  • High boiling point
  • High chemical stability
  • High flash point
  • High solvency
  • Low polarity
  • Low reactivity

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.993 g/cc0.0359 lb/in³
Molecular Weight 154 g/mol154 g/mol
Vapor Pressure 0.0462 bar34.7 torr
 
Thermal PropertiesMetricEnglishComments
Boiling Point 255 °C491 °F
Flash Point 113 °C235 °FASTM D92
 
Descriptive Properties
AppearanceClear colorless liquidAbove 69°C
 White solidBelow 69°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTOWAX® SH 105 Powder Paraffin Wax
Lithium Nitrate, LiNO3
MV Labs K500 KF Potassium fluoride
Methyl phenyl ether
Hong Kun Group UV 234 UV Absorber

PEATM5086 / 222280

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.