MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Hifax TRS 123D Black Thermoplastic Elastomeric Olefin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hifax TRS 123D Black medium melt flow, 1000 MPa flexural modulus, reactor grade thermoplastic elastomeric olefin (TEO) resin has an excellent balance of impact, stiffness, paintability, and processability that is typically used for all-terrain vehicle (ATV) components. It is based on material from Lyondell Basell’s proprietary Catalloy process.

Availability: North America

Application: Body Panels; Exterior Automotive Applications; Sports, Leisure & Toys

Market: Outdoor Equipment

Processing Method: Injection Molding

Attribute: Good Moldability; Good Processability; Good Stiffness; High Impact Resistance; High Shrinkage; Medium Flow; Paintable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³Method A; ISO 1183-1
Melt Flow 17.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
17.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psiISO 527-1, -2
Elongation at Yield 8.00 %8.00 %ISO 527-1, -2
Flexural Modulus 1.00 GPa145 ksiISO 178
Gardner Impact 25.4 J
@Temperature -30.0 °C
18.7 ft-lb
@Temperature -22.0 °F
Geometry GC; ASTM D5420
Impact Test 25.0 J
@Temperature -30.0 °C
18.4 ft-lb
@Temperature -22.0 °F
Multi-axial Impact Strength, (2.2 m/s, 3.2 mm plaque), Energy at max load, ductile failure); ASTM D3763

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9161 / 324096

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.