MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
Plansee MLR Molybdenum-Lanthanum Oxide; Recrystallized Sheet
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal

Material Notes: Characteristics:
  • "Stacked fiber" microstructure
  • Extremely creep resistant

Applications:

  • Furnace components - wires, including stranded; sintering and annealing boats; evaporator coils
  • Lighting - retaining and feed wires

Information provided by Plansee.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers <= 230
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 2000 °CMicrostructure stable up to this point
 
Component Elements PropertiesOriginal ValueComments
Molybdenum, Mo 99.3 %Balance
Other, each 0.70 %Lanthanum Oxide
 
Descriptive Properties
Creep Resistance< 1400°Cmuch greater than pure Mo
Ductilitymuch greater than pure Moafter HT use
Recrystallization Temperaturemuch greater than pure Mo
Stability at High Temperature> 1400°Cgreater than pure Mo
Stability at Room Temperaturecomparable with pure Mo
Weldabilitygreater than pure Mo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plansee ML MoLa2O3 stress relieved sheet
Plansee TZM sheet
Molybdenum, Mo, Recrystallized
Overview of materials for Molybdenum Alloy
Molybdenum, Mo, Annealed

NPLAM904 / 135460

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.