MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant and Cu-inhibitor should be added to meet specific ageing requirements.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • LV silane cross-linking insulation – 2 step process

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.931 g/cc0.0336 lb/in³ExxonMobil method
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength at Break 11.7 MPa1700 psiASTM D638
Tensile Strength, Yield 15.2 MPa2200 psiASTM D638
Elongation at Break 510 %510 %ASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus, 1% Secant 379 MPa55000 psiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cmASTM D257
Dielectric Constant 2.2
@Frequency 60 Hz
2.2
@Frequency 60 Hz
STM D150
Dielectric Strength 63.0 kV/mm1600 kV/in50 V/sec; ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 116 °C<= 241 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX99281 / 175517

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.