MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ COLORCOMP™ Compound A1000PXB Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: LNP COLORCOMP A1000PXB compound is based on unfilled Acrylonitrile Butadiene Styrene (ABS) resin. Added features of this grade include: Healthcare, Biocompatible (ISO10993), Low Extractables, Gamma & EtO Sterilizable, Exceptional Processing.

Features: Low Extractable,Aesthetics and Appearance,Healthcare,Steam, Gamma, EtO and E-beam sterilizable,Custom Color,Food Contact Acceptable,Exceptional Processing,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Moisture Absorption 0.100 %0.100 %Injection Molding
Viscosity 173000 cP173000 cPmelt; ISO 11443
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  11.7 g/10 min
@Load 3.80 kg,
Temperature 230 °C
11.7 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 12 g/10 min
@Load 5.00 kg,
Temperature 220 °C
12 g/10 min
@Load 11.0 lb,
Temperature 428 °F
ISO 1133
 42 g/10 min
@Load 10.0 kg,
Temperature 220 °C
42 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psi5 mm/min; ASTM D638
 35.0 MPa5080 psi5 mm/min; ISO 527
Tensile Strength, Yield 40.0 MPa5800 psi5 mm/min; ISO 527
 46.0 MPa6670 psi5 mm/min; ASTM D638
Elongation at Break 18 %18 %5 mm/min; ASTM D638
 35 %35 %5 mm/min; ISO 527
Elongation at Yield 2.0 %2.0 %5 mm/min; ASTM D638
 2.0 %2.0 %5 mm/min; ISO 527
Tensile Modulus 2.45 GPa355 ksi1 mm/min; ISO 527
 2.48 GPa360 ksi5 mm/min; ASTM D638
Flexural Strength 70.0 MPa10200 psiyield, 2 mm/min; ISO 178
 79.0 MPa11500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
 2.62 GPa380 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 240 J177 ft-lbASTM D256
 80.0 J
@Temperature -30.0 °C
59.0 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.30 J/cm²10.9 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 21.0 J15.5 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VUL 746A
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness >=1.50 mm
7.0 - 15 sec
@Thickness >=0.0591 in
UL 746A
 15 - 30 sec
@Thickness >=3.00 mm
15 - 30 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness >=1.50 mm
15 - 30 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 88.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
@Thickness 3.20 mm
199 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 77.0 °C
@Thickness 3.20 mm
171 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 98.0 °C208 °FRate B/50; ASTM D1525
 98.0 °C208 °FRate B/50; ISO 306
 100 °C212 °FRate B/120; ISO 306
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
Glow Wire Ignition Temperature  700 °C
@Thickness 1.00 mm
1290 °F
@Thickness 0.0394 in
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-13
 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  650 °C
@Thickness 1.00 mm
1200 °F
@Thickness 0.0394 in
IEC 60695-2-12
 650 °C
@Thickness 1.50 mm
1200 °F
@Thickness 0.0591 in
IEC 60695-2-12
 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-12
 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 205 - 245 °C401 - 473 °F
Zone 2 200 - 210 °C392 - 410 °F
Zone 3 205 - 225 °C401 - 437 °F
Melt Temperature 205 - 245 °C401 - 473 °FInjection Molding
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 70 %50 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80519 / 288466

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.