General purpose, reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated R190H-N3; Black: Designated R190HB. Data provided by the manufacturer |
Ashley Polymers, Inc.; Polyoxymethylene (POM) |