MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Radici Heraflex® E 6521 TPC-ET Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: TPC-ET Thermoplastic Elastomer. Medium-high Modulus, Nominal Shore D/15s 57. Natural color

Processing technology: Injection molding

Information provided by Radici group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/cc
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
MI / 08
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 230 °C
23 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565Instantaneous; ISO 868
 57
@Time 15.0 sec
57
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 49.0 MPa7110 psiISO 527-1/2
Elongation at Break 634 %634 %ISO 527 1/2
Flexural Modulus 0.342 GPa49.6 ksiISO 178/1A
Izod Impact, Notched NBNBASTM D256
Tear Strength 241 kN/m1380 pliASTM D1004
Abrasion 2020mm3; DIN 53516
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Melting Point 210 °C410 °F
Vicat Softening Point 195 °C
@Load 5.10 kg
383 °F
@Load 11.2 lb
50°C/h
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 722 Low Density Polyethylene (LDPE)
BASF Elastollan® SP 883 TPUR

PRADI753 / 120266

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.