MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lehvoss LUVOCOM® 3-8266/BL Polyamide 6 unreinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Properties/attributes include: Improved friction and wear behavior. Emergency (dry) running property. Isotropic shrinkage characteristics. Applicable e.g. for machine parts, moulds, tools and containers used in the food industry. Detectable.

Automotive industry, textile machinery, apparatus- and precision engineering. Typical uses include: Reduced moment of inertia compared with metal parts.

Processing: During processing the moisture level should not exceed 0.1%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. Excessively high predrying temperatures may cause discoloration. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.69 g/cc1.69 g/ccISO 1183
Moisture Absorption <= 1.00 %
@Temperature 23.0 °C,
Time 86400 sec
<= 1.00 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.011 - 0.015 cm/cm0.011 - 0.015 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 65.0 MPa9430 psiISO 527-2
Elongation at Break 2.3 %2.3 %ISO 527-2
Modulus of Elasticity 4.50 GPa653 ksiISO 527-2
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 3.80 GPa551 ksiISO 178
Flexural Strain at Break 3.0 %3.0 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+10 ohm-cm>= 1.00e+10 ohm-cmIEC 60167
Surface Resistance >= 1.00e+10 ohm>= 1.00e+10 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °FContinuous; UL 746B
 120 °C248 °FShort Term
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 280 °C518 - 536 °F
Zone 1 250 - 270 °C482 - 518 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 270 °C518 °F
Mold Temperature 70.0 - 110 °C158 - 230 °F
Drying Temperature  75.0 °C
@Time 36000 - 57600 sec
167 °F
@Time 10.0 - 16.0 hour
Dehumidifying dryer
 105 °C
@Time 14400 - 21600 sec
221 °F
@Time 4.00 - 6.00 hour
Dehumidifying dryer
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Colorsapphire blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8916 / 193875

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.