MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROCHEM® DDCBP-50 Cross-linking agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Akrochem DDCBP-50 is a white, stiff paste consisting of 50% Di(2,4-dichlorobenzoyl)peroxide, desensitized with silicone oil. This halogenated diaryl peroxide is used as a source of radicals in the cross-linking of polymers above 100°C, primarily silicone rubber.

Applications: Akrochem DDCBP-50 peroxide is used as a catalyst for cross-linking a variety of synthetic rubbers, primarily silicone; at temperatures above 100°C (100-115°C cures should be done under pressure and then post-cured 12-24 hrs. at 150-250°C). Typical usage level is 1-2 phr of product as supplied. DDCBP-50 has the lowest activation temperature and the highest rate of cure of any of the common peroxides used in cross-linking. It is ideally suited for fast curing of thin cross-sections in continuous cures. Special advantages of this peroxide: Not oxygen inhibited. Can be used in hot air cures at atmospheric pressures at temperatures from 150-250°C. Decomposition products have a very low vapor pressure so porosity does not normally occur. Has FDA acceptability under regulation 177.2600, rubber articles in repeated contact with food. Disadvantages: Caution must be used in dealing with the fast scorch times. The peroxide is sensitive to carbon blacks. Also, thick cross-sections may revert due to acid by-products of decomposition. Another use of DDCBP-50 is in combination with other peroxides. This may allow de-molding of parts that would otherwise hot tear by first curing with the DDCBP-50 before the second peroxide becomes active. Post-curing then finishes cure.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/cc
 
Descriptive Properties
AppearanceStiff, white paste
Content2.06-2.15%Active Oxygen
 49-51%Di(2,4-Dichlorobenzoyl)peroxide
Half-Life Thermal Decomposition Data1 hrs72°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH560 / 315478

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.