Hifax TRC 1230P JA6A Black thermoplastic polyolefin is typically used for automotive and heavy-truck applications that require energy management combined with ductility, stiffness and impact resistance over a broad temperature range. This material exhibits excellent processability and dimensional stability. Status: Developmental Availability: North America Application: Automotive Parts; Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Information provided by LyondellBasell. |