MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Lushan EV1050G2 EVA Film for Encapsulating Solar modules, High Transmittance
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemical Accessories. EVA film for encapsulating solar modules Lushan series could effectively protect to the PV cell, and has excellent performance of transmittance and ageing-resistant. It provides structural support, electrical isolation, physical isolation/protection, and thermal conduction for solar circuits, as well as to maximize the service life of solar module. Solar EVA Film Characteristic:
  • High volume resistivity and lasting adhesion strength holding capacity, and insure PV modules have long service life
  • Low yellowness index change and low light transmittance attenuation, insure the high service efficiency of PV modules
  • Excellent compatibility with flux, welding ribbon, location tap, backsheet and silica gel
  • Solar EVA film quality stability ensured by the complete and scientific quality management system.

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 1183
Water Absorption <= 0.10 %ISO 62:2008
Melt Flow 17 - 27 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15.0 MPaISO 527-3
Elongation at Break >= 500 %
Tensile Modulus 5.00 MPaYoung's; ISO 527-3
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 65.0 - 75.0 °CASTM D148
Shrinkage, MD 0.00 %
@Temperature 120 °C,
Time 180 sec
Q/LSXC
Shrinkage, TD 0.00 %
@Temperature 120 °C,
Time 180 sec
Q/LSXC
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ISO 489
Yellow Index 5.6 %
@Time 0.000 sec
after heat and humidity aging (85°c, 85 RH%)
 5.8 %
@Time 0.000 sec
 5.9 %
@Time 2.88e+6 sec
 5.9 %
@Time 2.88e+6 sec
after heat and humidity aging (85°c, 85 RH%)
 6.0 %
@Time 3.24e+6 sec
after heat and humidity aging (85°c, 85 RH%)
 6.3 %
@Time 3.60e+6 sec
 8.0 %
@Time 7.20e+6 sec
 8.2 %
@Time 7.20e+6 sec
after heat and humidity aging (85°c, 85 RH%)
UV Transmittance >= 91 %ASTM D1003
 
Descriptive Properties
Surface UncuredOne Side Embossed
Thickness Tolerance±0.02Q/LSXC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Innospec FLEXAREN® 14003 EVA-Copolymer
Innospec FLEXAREN® 14001 EVA-Copolymer
Innospec FLEXAREN® 09009 EVA-Copolymer
Innospec FLEXAREN® 09002 EVA-Copolymer
Innospec FLEXAREN® 07002 EVA-Copolymer

PLUSH012 / 150010

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.