MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GOYENCHEM-OBSH 4,4'-Oxybis(benzenesulfonyl hydrazide)(OBSH) High Effective Foaming Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No.80-51-3

Intro: GO YEN CHEMICAL INDUSTRIAL CO,. LTD. (GYC Group) as Taiwan’s most innovative manufacturer of functional fine CHEMICAL products, accomplished with strong R&D team aim for current problems in the industries providing the total solution for newly generation products. GOYENCHEM-OBSH 4,4'-Oxybis(benzenesulfonyl hydrazide) (OBSH) is a kind of highly efficient foaming agent, especially as the replacement of traditional AC foaming agent overcome its disadvantage and problems as the newly type formulation. It can be widely used in rubber, plastic, foam, wire and cable industry with good insulation. OBSH belongs to Sulfonyl Hydrazide as the most common use foaming agent. It can also combine with other foaming agent who is appointed by the most renown companies as the standard formula.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 6.0 - 8.06.0 - 8.0
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 158 - 164 °C316 - 327 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Descriptive Properties
Amount of Generating Gas125-140 ml/g
AppearanceWhite Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN357 / 266665

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.