MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem Antioxidant 12
Categories: Other Engineering Material

Material Notes: Product Description: Antioxidant 12 is a sterically hindered polymeric phenol-type non-staining, non-discoloring antioxidant. It is used as a stabilizer and antioxidant in a variety of polymers, including natural and synthetic polyisoprene, neoprene, nitrile, styrene butadiene and latex. Antioxidant 12 complies with 21 CFR FDA Regulations 175.105 (Adhesives) and 177.2600 (Rubber Articles).

Application: Antioxidant 12 is extremely active and persistent due to low volatility and low extractability. It remains active and stable indefinitely and does not hydrolyze. Antioxidant 12 effectively inhibits degradation of polymers due to heat and oxygen. Color development in polymers is inhibited by improved thermal stability, reducing scorch, and by oxidative and UV stability (A.O. 12 is not considered a UV stabilizer but will yellow less than comparable antioxidants under UV exposure). The excellent thermal stability makes Antioxidant 12 useful in hot melt adhesives. Antioxidant 12 is also available as an aqueous dispersion for use in latex and latex foam under the name Akrosperse W-9924 AO 12 (50%).

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
Volatiles <= 2.0 %
@Temperature 150 °C,
Time 7200 sec
<= 2.0 %
@Temperature 302 °F,
Time 2.00 hour
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 105 °C>= 221 °F
 
Descriptive Properties
AppearanceCream Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH483 / 315401

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.