MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergadur™ PB40 G30 UF UV Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³±0.03 g/cm³; DIN 53479
Filler Content 30 %30 %Glass Fiber Reinforcement
Melt Index of Compound 14 g/10 min
@Load 1.60 kg,
Temperature 250 °C
14 g/10 min
@Load 3.53 lb,
Temperature 482 °F
cm³/10min; ISO 1133
Ash 30 %30 %ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.0 MPa
@Temperature 23.0 °C
13100 psi
@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 2.5 %
@Temperature 23.0 °C
2.5 %
@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 8.20 GPa
@Temperature 23.0 °C
1190 ksi
@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched 7.40 J/cm²
@Temperature 23.0 °C
35.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 224 °C435 °FISO 3146
Maximum Service Temperature, Air 140 °C284 °FContinuous (GTP 50% Tensile); IEC 60216
 170 °C338 °FShort Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 225 °C437 °FUnannealed; ISO 75-2/B
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Internal Method
Glow Wire Ignition Temperature 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-13
 
Descriptive Properties
AdditiveUV Stabilizer
FeaturesFlame Retardant
 Halogen Free
 Low (to None) Phosphorus Content
FormsPellets
Generic MaterialPBT
Generic NamePolybutylene Terephthalate (PBT)
Regional AvailabilityAfrica & Middle East
 Europe
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT)
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Celanese Celanex® 2300 GV1/30 PBT, 30% Glass Reinforced
Avient Bergadur™ PB400 G30 H UF UV Polybutylene Terephthalate (PBT)

PH0POL0772 / 145341

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.