MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AdvanSource Biomaterials ChronoFlex® AR Biodurable Medical Grade Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polycarbonate (PC); Polyurethane, TP; Polycarbonate-Urethane

Material Notes: AdvanSource Biomaterials Corporation manufactures and markets this solution-grade, segmented, aromatic, polycarbonate-based polyurethane designed for use in solvent casting and dipping applications. This elastomer may be evaluated for use in the fabrication of blood contact surfaces, pump diaphragms, and other medical devices. Exceptional flexure endurance leads to uses such as artificial heart diaphragms or vascular grafts.

Synthesis of ChronoFlex® AR is carried out by the addition of MDI (diphenylmethane 4,4'-diisocyanate) to polycarbonate diol, followed by addition of a mixture of chain extenders and a molecular weight regulator, with the reaction carried out in DMAC solvent. ChronoFlex® AR is thus supplied as a 22% solids solution, ready for solution casting.

Information provided by AdvanSource Biomaterials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D2240
Tensile Strength, Ultimate 7500 psiFilm; ASTM D412
Elongation at Break 500 %Film; ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane
Titanium Ti-6Al-4V (Grade 5), Annealed
AdvanSource Biomaterials HydroMed™ D640 Permanently Lubricious Polyurethane Coating

PCARDI03 / 27927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.