MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Almaak Anjacom® PA6 255-UV/GF30 Nylon 6, 30% Glass Fiber Reinforced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: reinforced, 30% glass fiber, UV stabilized

Information provided by Almaak International GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Filler Content 30 %30 %
Water Absorption 7.5 %7.5 %ISO 62
Moisture Absorption 2.30 %2.30 %50% RH; ISO 62
Viscosity Number 145 cm³/g1.45 dl/gISO 307
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.0090 cm/cm0.0080 - 0.0090 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 170 MPa24700 psi5 mm/min; ISO 527-1/2
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527-1/2
Modulus of Elasticity 9.00 GPa1310 ksi1 mm/min; ISO 527-1/2
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F
Deflection Temperature at 0.46 MPa (66 psi) 212 °C414 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FISO 75
Vicat Softening Point 203 °C
@Load 5.10 kg
397 °F
@Load 11.2 lb
50K/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 - 10.0 hour4.00 - 10.0 hour
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Quality levelRecycleDIN EN ISO 14021
Recycled content (Polymer)>80%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLMA9830 / 316458

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.