MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives TURBO FUSE SERIES 180 BLACK TOUGHENED (2400 Viscosity) Rapid Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 143 – BLACK TOUGHENED advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications. The fast curing qualities make it especially desirable in high speed industrial production. TURBO FUSE SERIES 143 is ideal for use in applications that require an easily handled medium viscosity adhesive. Because of the 300 viscosity, it works especially well in close to medium fitting applications such as unfinished metal to metal bonding, metal to rubber, and rubber to rubber, such as "O" ring repair/manufacture. The BLACK TOUGHENED formula is especially good for sound speakers. Because of the 2400 viscosity, it works especially well in bonding porous surfaces like ceramics, and is excellent for bonding metal and rubber parts. The BLACK TOUGHENED formula is especially good for sound speakers.

Part Numbers for this data: 04-143B, 10-143B, 15-143B, 20-143B, 25-143B, 30-143B, 35-143B

Soluble in Acetone, MEK, Amide, Methylene Chloride

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 7085-85-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccLiquid State
Viscosity 2300 - 2500 cPLiquid State
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 65Cured State
Shear Strength 2500 psiTensile, (Cured State)
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.33
@Frequency 1e+6 Hz
Cured State
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °FCured State
Softening Point 330 °FCured State
Minimum Service Temperature, Air -65.0 °FCured State
Flash Point 170 - 200 °FLiquid State
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 MonthLiquid State
 
Descriptive Properties
AppearanceBlack LiquidLiquid State
 Black-HardCured State
Base compound (Resin)Ethyl CyanoacrylateLiquid State
Gap Fill0.008"Cured State
Material Set Up Time10-30 secRubber to Rubber
 15-30 secAluminum to Aluminum
 40-100 secSteel to Steel
 50-80 secPolycarbonate to Polycarbonate
 50-90 secPhenolic to Phenolic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive
Permabond 737 Cyanoacrylate, toughened
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Henkel Loctite® 480 Toughened Ethyl Cyanoacrylate Bonding Adhesive
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy

PPALML023 / 135177

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.