MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotchcast™ 3570G-N Connector Sealing Pack
Categories: Polymer; Thermoset

Material Notes: The 3M Scotchcast Connector Sealing Pack 3570G-N insulates and provides protection for electrical spring connectors against dust, soil, water, and other environmental elements. Each sealing pack contains a specific amount of the two-part 3M Scotchcast Epoxy Resin 3570G-N in a unique closed mixing pouch. The resin generates its own heat to cure and its compatibility with spring connectors makes this sealing pack a convenient insulating and encapsulating resin for electrical spring connections. The 3570G-N sealing pack will accommodate one 3M Performance plus Wire Connector O/B, R/Y, T/R, T/Y or one 3M Electrical Spring and Grounding Connector 312 or 512.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D2240
Tensile Strength at Break 12.3 MPa1780 psiASTM D638
Elongation at Break 57 %57 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.2
@Frequency 60.0 Hz,
Temperature 23.0 °C
2.2
@Frequency 60.0 Hz,
Temperature 73.4 °F
ASTM D150
 8.9
@Frequency 60.0 Hz,
Temperature 90.0 °C
8.9
@Frequency 60.0 Hz,
Temperature 194 °F
ASTM D150
Dielectric Strength 17.1 kV/mm435 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 21.0 °C69.8 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 8.00 - 12.0 min8.00 - 12.0 minASTM D24799
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35237 / 169984

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.