MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Go Yen Chemical GY-LU100 Dispersing Slip Agent For PVC & Paint
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • GY-LU100 provide excellent flow properties
  • Excellent processing PVC processing aid
  • GY-LU100 can be applied on different kinds of extrusion and injection products
  • Applied on PVC pipe & film
  • Provide highly lubricant property of plastic
  • Enhance the property of dispersing
  • Improve the processing properties toward the resin of paint and coating
  • Accomplished with well electric ability & chemical resistance
  • Well ability of lubrication to act as plastic lubrication
  • Can enhance the flow properties of Polyethylene, polypropylene, ABS; the property of mold release ofpolymethyl methacrylate, polycarbonate while acting as the release agent
  • Perfect light fastness toward TGIC polyester powder coatings
  • Can be applied as the adjustment of melt flow rates.
  • The impact resistant strength and softening properties can be enhanced while applying in the painting such as
  • Polyester resin / epoxy resin / matting curing agent.
  • GY-LU100 can improve the surface flatness and anticrack toward powder coating paint
  • Applied on other plastic and rubbery product
  • As the lubrication and dispersion agent for plastic masterbatch
  • Processing modifier of plastic and elastomers, also applied on ink modification and paper layer and candle etc.
Applications:
  • polyethylene / polypropylene/ ABS
  • PVC pipe & frame
  • Irregular shaped materials
  • poly (methyl methacrylate) / polycarbonate
  • high light curing TGIC polyester powder coating
  • polyester resin / epoxy resin / matting curing agent
  • Film and other plastic and rubbery processing items
  • Plastic masterbetch dispersing agent and lubrication agent
  • Processing aid of plastic and elastomers
  • Polishing agent for ink
  • For paper layer
  • candles

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.050<= 0.050[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Softening Point <= 105 °C<= 221 °F
 
Descriptive Properties
AppearancePowder form
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN399 / 266707

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.