MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Superwool® Inorganic Bonds and Shapes I-Superwool HT H Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: AES fiber class. Inorganic fiber grade. Superwool inorganic boards are processed from a slurry consisting of Superwool bulk fiber and inorganic binders. Boards up to 36” wide may be ordered with both surfaces machined smooth to a close thickness tolerance. Superwool is a low bio-persistent fiber, manufactured from pure raw materials and processed to offer excellent performance in high-temperature applications. Superwool offers an alternative to traditional solutions due to its high refractoriness and excellent non-wetting characteristics with molten aluminum. Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalis (e.g. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying. Superwool is ideally suited to individual applications and is available in a wide range of thicknesses and densities. The maximum continuous use temperature depends on the application.

Applications:

  • Molten aluminum contact
  • Furnace, kiln, and oven hot face linings
  • Flue and chimney linings
  • Insulation as backup to:
    • firebrick
    • insulating firebrick
    • refractory castables
    • rammed shapes
  • Appliance and heat processing insulation.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.742 g/cc
Loss On Ignition 3.1 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00286 GPa
Compressive Strength 0.410 MPaat 5% deformation
 0.670 MPaat 10% deformation
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 1177 °CContinuous Use
Shrinkage 1.0 %
@Treatment Temp. 816 °C,
Time 86400 sec
 2.5 %
@Treatment Temp. 982 °C,
Time 86400 sec
 2.7 %
@Treatment Temp. 1093 °C,
Time 86400 sec
 2.8 %
@Treatment Temp. 1204 °C,
Time 86400 sec
 
Component Elements PropertiesOriginal ValueComments
CaO 5.0 %
Other >= 1.0 %
SiO2 94 %
 
Descriptive Properties
Classification Temperature (°C)1275
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6502 / 203286

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.