MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lehvoss LUVOCOM® 1-1108 Nylon 66, Carbon Fiber Filled, heat stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Carbon Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Polyamide 66 with carbon fibers, heat stabilized, natural color (black)

Main features: Very strong and stiff parts; low coefficient of thermal expansion. Reduced moment of inertia compared with metal parts. Electrically conductive, suitable for continuous discharging of statically-generated electricity. Low warpage.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccISO 1183-3
Water Absorption <= 1.00 %
@Time 86400 sec
<= 1.00 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.00300 - 0.00800 cm/cm0.00300 - 0.00800 in/inDIN 16742
Melt Flow 30.0 g/10 min
@Load 2.16 kg,
Temperature 285 °C
30.0 g/10 min
@Load 4.76 lb,
Temperature 545 °F
pellet
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 160 MPa23200 psi50 mm/min; ISO 527
Elongation at Break 4.00 %4.00 %50 mm/min, Fmax; ISO 527
Tensile Modulus 10.0 GPa1450 ksi1 mm/min; ISO 527
Flexural Strength 235 MPa34100 psi10 mm/min; ISO 178
Flexural Modulus 8.50 GPa1230 ksi2 mm/min; ISO 178
Flexural Strain at Break 4.20 %4.20 %10 mm/min, Fmax; ISO 178
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
80x10x4mm; ISO 179 1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm; ISO 179 1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²80x10x4mm; ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1e+05<= 1e+05Ronde 60x4mm; DIN EN 62631-3-2
Insulation Resistance <= 100000 ohm<= 100000 ohmstrip electrode R25; DIN EN 62631-3-3
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air  110 °C
@Time 7.20e+7 sec
230 °F
@Time 20000 hour
Continuous; IEC 60216
 160 °C
@Time 720000 sec
320 °F
@Time 200 hour
during lifetime
Vicat Softening Point 245 °C473 °FVST A; DIN ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 300 °C536 - 572 °F
Zone 1 290 - 310 °C554 - 590 °F
Zone 2 290 - 310 °C554 - 590 °F
Zone 3 290 - 310 °C554 - 590 °F
Melt Temperature 290 °C554 °F
Mold Temperature 90.0 - 120 °C194 - 248 °F
Drying Temperature  75.0 °C
@Time 21600 - 57600 sec
167 °F
@Time 6.00 - 16.0 hour
Dehumidifying
 105 °C
@Time 14400 - 21600 sec
221 °F
@Time 4.00 - 6.00 hour
Vacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8701 / 325085

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.