Hostacom ERC 213N 2 C12827 is a 15% talc filled PP copolymer, with good flowability, excellent impact/stiffness balance and excellent scratch resistance. The product is also available as a customized color matched, pellet form. This grade is delivered in C12827 color version. Applications : Instrument Panels.Information provided by LyondellBasell. |