MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Terves TervAlloy™ 3143 (HD) Dissolvable Magnesium Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: TervAlloy™ 3143 (HD) is a special high ductility version of Terves’ patented dissolvable magnesium designed for oil and gas applications. This material is based on our TervAlloy™ 3241 (TAx100E) product offering, and demonstrates similar dissolution rates in potassium chloride and sodium chloride brine solutions. TervAlloy 3143 is designed for higher ductility applications – allowing greater flexibility to meet the needs of specific customer applications. This product can be purchased in one inch increments in lengths up to 48 inches (depending on shape).

Information provided by Terves Incorporated

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 39.6 ksi4" Solid Rod, 5:1 Extrusion Ratio
Tensile Strength, Yield 24.2 ksi4" Solid Rod, 5:1 Extrusion Ratio
Elongation at Break 16 %4" Solid Rod, 5:1 Extrusion Ratio, Longitudinal values
Compressive Strength 57.5 ksi4" Solid Rod, 5:1 Extrusion Ratio
Shear Strength 19.5 ksi4" Solid Rod, 5:1 Extrusion Ratio
 
Descriptive Properties
Dissolution Data14 mg/cm2hr1.0% KCl, 60°C
 17 mg/cm2hr3% KCl, 60°C
 2 mg/cm2hr1.0% KCl, 30°C
 2 mg/cm2hr3% KCl, 30°C
 20.5 mg/cm2hr8% KCl, 60°C
 33 mg/cm2hr3% KCl, 90°C
 39.9 mg/cm2hr3.5% NaCl, 90°C
 48.4 mg/cm2hr3.5% NaCl, 90°C
 69 mg/cm2hr1.0% KCl, 90°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTERVES014 / 314481

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.