MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Novec™ FC-4434 Fluorosurfactant
Categories: Fluid

Material Notes: 3M™ Novec™ Fluorosurfactant FC-4434 is a water-soluble, general purpose nonionic fluorinated surfactant which contributes excellent wetting, spreading and leveling properties to a variety of coating systems. Some typical application areas include architectural coatings, inks, floor polishes, high solids coatings, water reducible coatings and radiation curable coatings.

Suggested Applications: Novec fluorosurfactant FC-4434 is a dilute solution of 25% active fluorochemical surfactant in a water miscible diluent. It may be used as a flow and leveling agent in various applications including, inks, paints and coatings, polymers, adhesives, waxes, polishes and caulks. Recommended use level is between 0.05% and 0.3% active surfactant. However, use level can vary depending on the application and concentration of other additives and solvents in the formulation.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.006 g/cc1.006 g/cc
Density 1.01 g/cc0.0364 lb/in³
Solubility in Water 1.0 %1.0 %
pH 4.54.5of 1% aqueous solution
Viscosity 14 cP14 cP
Vapor Pressure 0.002657 bar
@Temperature 55.0 °C
1.993 torr
@Temperature 131 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 78.0 °C172 °FSetaflash closed cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.431.43
Gardner Color Number 2.2 - 2.72.2 - 2.7
 
Descriptive Properties
AppearanceClear yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 7100DL Engineered Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 7000 Engineered Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 71DA Engineered Fluid

PMM40001 / 194892

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.