Features:- UL 94 V-0 @ 1.6mm
- Low smoking, low halogen
- Excellent balance properties, high strength
- Excellent heat stability
- Excellent electrical properties
Applications:- Injection molding
- Gas molding
- TV or audio housing
- Electrical appliance housing
Information Provided by Kingfa Sci. & Tech. Co., Ltd. |