MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay GEROPON® TC 42 LQ Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Liquid Sodium Methyl Cocoyl Taurate that demonstrates good lathering properties in skin cleanser and shampoo applications. Displaysexcellent dispersiblity properties in hard water and high electrolyte loads

Chemical Name: SODIUM N-COCONUT ACID-N-METHYL TAURATE

CAS: 61791-42-2; 61788-47-4; 7732-18-5

Biodegradability: Readily biodegradable, Closed Bottle >80% in 28 days

Available in: Asia Pacific, Europe, Latin America and North America

Applications: GEROPON® TC-42 LQ is a liquid anionic surfactant with excellent solubility and outstanding detergency and wetting properties coupled with dispersing and suspending action. It is stable in high electrolyte systems, mild acids and is mild to hair and skin. GEROPON® TC-42 LQ exhibits excellent lathering properties similar to fatty acid soaps. Unlike soaps, GEROPON® TC-42 LQ is stable in mildly acidic systems and displays good performance properties in hard water solutions.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 70 %by Volume
pH 6.0 - 7.0as is @25°C; RP-0420
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceClear to Cloudy LiquidMay Precipitate Upon Storage, RP0064
Color<200APHA, RP-0134
CompositionActive33-36%, EQ. WT. 363, RP-0027
 Free Fatty Acid<5.0%, RP-0971
OdorTypical Fatty

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay GEROPON® T/36 DF Surfactant
Solvay GEROPON® SS OIP LPH Surfactant
Solvay GEROPON® SDS Surfactant
Solvay GEROPON® TA/72 Surfactant
Solvay GEROPON® T-22 A Surfactant

WRHOD137 / 137368

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.