MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Sika SikaBond® Construction Adhesive One part advanced polyurethane, elastomeric adhesive
Categories: Polymer; Adhesive

Material Notes: SikaBond Construction Adhesive is a one-component, gun-grade, adhesive and sealing compound of permanent elasticity. This dual-purpose material is based on a special moisture-cured polyurethane with an accelerated curing time.

Where to Use As an elastic adhesive for:

  • Paver caps, masonry veneer and Faux stone.
  • Cover plates, gaskets and coverings.
  • Acoustic ceiling tiles.
  • Floor moldings and door sills.
  • Light weight construction materials.
  • Wood, metal, or plastic window and door frames.
  • Roof tiles.
As an elastic joint sealer for:
  • Air ducts and high vacuum systems.
  • Containers, tanks, and silos.
  • Gaskets in openings in walls or floors for ducts, piling, etc.
  • Reservoirs or water retaining structures.
  • Aluminum fabrication.
  • Bolted lap joints.
Advantages:
  • Excellent adhesion on all cement-based materials, brick, ceramics, glass, metals, wood, epoxy, polyester, acrylic resin, and plastics.
  • Fast cure rate.
  • Waterproof and water immersible after cure.
  • Good weathering resistance.
  • Non-corrosive.
  • Can be painted over with water, oil, and rubber-based paints. (Preliminary tests recommended).
  • High durability.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 76.7 °C170 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 37.8 °C40.0 - 100 °FApplication Temp; Condition material to 65°-75°F before using.
Cure Time 4320 - 7200 min72.0 - 120 hourFinal Cure
Shelf Life 12.0 Month
@Temperature 4.44 - 26.7 °C
12.0 Month
@Temperature 40.0 - 80.1 °F
in original unopened cartridge
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asia Technology Pioneers CAP 102 PP Nanocomposite

PSIKA917 / 209824

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.